D862 cobalt base electrode
use:
Used for surfacing welding high temperature work under the service of burning single roller crusher tooth crown grate board and blast furnace rotating cloth chute, wear-resistant effect is remarkable.
Deposited metal chemical composition (%)
| C | Mn | Si | S | P | Cr | Ni | Fe | W | Cu | Co | Other elements of the total |
guarantee value | 0.20 / 0.50 | 1.45 | 2.00 | - | - | 9.00 / 15.00 | - | 9.00 | 20.00 | - | margin | ≤4.00 |
Surfacing layer hardness:
Reference current (AC, DC + )
Electrode diameter (mm) | φ2.5 | φ3.2 | φ4.0 | φ5.0 |
Welding current (A) | 50 ~ 100 | 70 ~ 130 | 100 ~ 160 | 140 ~ 200 |
Precautions:
⒈ welding electrode to be 300 ℃ baking 1h.
⒉ as much as possible the use of DC power supply, the current should not be too large.
related articles
The number of clicks:Update time:2017/12/26 19:06:54【print this page】