J506R
Description:
J502NiCu titanium calcium type coating of low alloy weathering electrode. AC and DC dual-use, can be all-position welding. Has excellent welding performance and mechanical properties, stable arc, spatter, easy slag removal; weld appearance, deposited metal has good resistance to atmospheric corrosion.
use:
Mainly used for weathering of the railway rolling stock welding, such as 09MnCrPTi and so on.
Deposited metal chemical composition (%)
| C | Mn | Si | S | P | Ni | Cu |
guarantee value | ≤0.12 | 0.30 ~ 0.90 | ≤0.40 | ≤0.030 | ≤0.035 | 0.20 ~ 0.50 | 0.20 ~ 0.50 |
Example value | 0.095 | 0.58 | 0.18 | 0.012 | 0.026 | 0.45 | 0.42 |
Deposited metal mechanical properties (welded)
Pilot projects | Rm (N / mm 2 ) | ReL / Rp 0.2 (N / mm 2 ) | A (%) | KV 2 (J) |
-40 ℃ |
guarantee value | ≥490 | ≥ 390 | ≥22 | ≥27 |
Example value | 540 | 450 | 27 | 73 |
X-ray inspection requirements:
Ⅱ level
Reference current (AC, DC)
Electrode diameter (mm) | φ2.5 | φ3.2 | φ4.0 | φ5.0 |
Welding current (A) | 60 ~ 90 | 80 ~ 130 | 140 ~ 200 | 180 ~ 240 |
Precautions:
Welding before welding must be removed rust, oil, water and other impurities.