J506NiCrCu
Description:
J506NiCu is a low hydrogen potassium type weathering steel electrode. AC and DC dual-use, can be all-position welding. The deposited metal has excellent resistance to atmospheric corrosion, crack resistance and good ductility and toughness.
use:
For carbon steel and 490N / mm 2 Welding Tensile strength level weathering steel, such as rolling stock welded structure, offshore engineering, bridges and the like.
Deposited metal chemical composition (%)
| C | Mn | Si | S | P | Ni | Cu |
guarantee value | ≤0.12 | 0.30 ~ 0.90 | ≤0.70 | ≤0.030 | ≤0.035 | 0.20 ~ 0.50 | 0.20 ~ 0.50 |
Example value | 0.060 | 0.82 | 0.19 | 0.008 | 0.016 | 0.35 | 0.30 |
Deposited metal mechanical properties (welded)
Pilot projects | Rm (N / m m2 ) | ReL / Rp 0.2 (N / mm 2 ) | A (%) | KV 2 (J) |
-40 ℃ |
guarantee value | ≥490 | ≥ 390 | ≥22 | ≥27 |
Example value | 530 | 450 | 27 | 166 |
X-ray inspection requirements:
Ⅰ level
Reference current (AC, DC + )
Electrode diameter (mm) | φ2.5 | φ3.2 | φ4.0 | φ5.0 |
Welding current (A) | 50 ~ 90 | 80 ~ 130 | 140 ~ 190 | 170 ~ 230 |
Precautions:
⒈ welding electrode to be baked by 350 ℃ 1h, with baking with the use.
⒉ weld before welding must be removed rust, oil, water and other impurities.
⒊ welding operation required to use a short arc to narrow the welding is appropriate.